MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Teijin Tenax® A HT P722 3mm Chopped carbon fiber
Categories: Carbon; Carbon Fiber/Carbon Fibre

Material Notes: Chopped carbon fiber in pelletized form is especially suited for volumetric, loss-in-weight, vibrating tray, screw, and other automated feeding operations in compounding.

Application: For use in high-temperature, thermoplastic resins where optimum mechanical and/or structural performance is required.

Chemical Identity: Carbon Fiber (PAN / polyacrylonitrile based)

Equivalent Raw Material(s): None

CAS Registry Number(s): 07440-44-0

Appearance: Dense, firm, elongated pellets with pointed ends and ovate in cross-section.

Information provided by Teijin Carbon America, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.425 g/cc0.0154 lb/in³
Density 1.79 g/cc0.0647 lb/in³
Volatiles 0.00 %0.00 %
Filament Diameter 7.0 µm7.0 µm
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 4400 MPa638000 psi
Tensile Modulus 232 GPa
@Strain 0.1 - 0.6 %
33600 ksi
@Strain 0.1 - 0.6 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

ETEIJIN926 / 277936

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.