MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Mateck Cadmium Telluride (CdTe)
Categories: Ceramic; Sulfide/Chalcogenide

Material Notes: Optical crystals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 5.86 g/cc
Solubility 0.00 ppm
a Lattice Constant 6.483 Å
Molecular Weight 240.01 g/mol
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity 52.0 GPa
Poissons Ratio 0.41
Shear Modulus 18.4 GPaCalculated
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.50 µm/m-°C
@Temperature 0.000 - 30.0 °C
Specific Heat Capacity 0.209 J/g-°C
Thermal Conductivity 4.10 W/m-K
Melting Point 1092 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 2.61n20.0
 2.649n10.0
 2.598
@Wavelength 22000 nm
 2.629
@Wavelength 16000 nm
 2.649
@Wavelength 10000 nm
 2.656
@Wavelength 6000 nm
IR Transmittance 10 %
@Wavelength 800 nm
Internal Transmittance
 15 %
@Wavelength 35000 nm
Internal Transmittance
 55 %
@Wavelength 950 nm
Internal Transmittance
 70 %
@Wavelength 15000 nm
Internal Transmittance
 
Descriptive Properties
Absorption loss (cm^-1)0.167at 10 microns
Symmetrycubic
Symmetry ClassF43m
Transmission Range (microns)2 - 25

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mateck CdTe
Cadmium Telluride, CdTe, Cubic
Cadmium Telluride, CdTe, Hexagonal
Aluminum 5083-H32; 5083-H323
Diamond, Synthetic

CMAT040 / 87724

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.