MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NovaCentrix Metalon® JS-B25P Nanosilver Inkjet Ink – Aqueous dispersion for Dimatix and Epson Printheads
Categories: Fluid; Other Engineering Material

Material Notes: JS-B25P is an electrically conductive ink designed to produce circuits on substrates such as Novele™ (PET with a microporous inkjet receptive coating) and photo paper. JS-B25P is specially formulated for compatibility and stability with piezo-inkjet printheads such as those used in Epson desktop printers and the Dimatix Samba system.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.30 g/cc1.30 g/cc
Solids Content 25 %25 %
Filler Content 25 %25 %Silver (Ag)
Particle Size 0.075 µm0.075 µm
 60 - 80 µm60 - 80 µmz-avg by DLS
Viscosity 3.0 - 5.0 cP3.0 - 5.0 cP
Thickness 0.200 - 1.00 microns0.00787 - 0.0394 mil
Surface Tension 28 - 32 dynes/cm28 - 32 dynes/cm
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 0.060 - 0.070 ohm0.060 - 0.070 ohmExample; on coated PET substrate
 
Processing PropertiesMetricEnglishComments
Cure Time 0.0000167 min2.78e-7 hourPhotonic Cure
 
Component Elements PropertiesMetricEnglishComments
Silver, Ag 25 %25 %
 
Descriptive Properties
Adhesion5B
Conductive Filler TypeSilver (Ag)
Material TypeReady-To-Use Formulation
Pencil Hardness>4H
Recommended SubstratesPorous, coated PET (Novele™)
Solvent SystemWater

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

ENOVA908 / 191518

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.