MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Abatron AboCast 8-3/Abocure 8-3 Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: 2-part solvent-free dielectric epoxy casting compound.

Processing: 100/50 ratio (pbw); Gel time, 100 g (3.5 oz.): 265 minutes; cures in 16 hours at 25°C (77°F); postcure: 2 hours at 100°C (212°F).

Applications: solventless casting, adhesive, and coating.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption 0.22 %0.22 %in 24 hours.
Viscosity Measurement 16001600
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8383
Tensile Strength, Ultimate 58.61 MPa8501 psi
Elongation at Break 5.5 %5.5 %
Flexural Strength 94.8 MPa13700 psi
Izod Impact, Notched 0.400 J/cm0.749 ft-lb/in
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  4.80e+11 ohm-cm
@Temperature 93.3 °C
4.80e+11 ohm-cm
@Temperature 200 °F
 6.20e+14 ohm-cm
@Temperature 65.6 °C
6.20e+14 ohm-cm
@Temperature 150 °F
 3.60e+15 ohm-cm
@Temperature 25.0 °C
3.60e+15 ohm-cm
@Temperature 77.0 °F
Dielectric Constant 3.33
@Frequency 1e+6 Hz
3.33
@Frequency 1e+6 Hz
Dissipation Factor 0.017
@Frequency 1e+6 Hz
0.017
@Frequency 1e+6 Hz
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 73.0 °C163 °FDeflection temperature; load unknown.
 
Processing PropertiesMetricEnglishComments
Processing Temperature 25.0 °C77.0 °FCuring time: 16 hours; Postcure: 2 hours/100°C (212°F)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CHT Group QSil 216 QSI Quantum Silicones Transparent Liquid Silicone Rubber
Mitsubishi Chemical Advanced Materials Ketron™ Sterra™ HPV PEEK Recycled poly-ether-ether-ketone
CHT Group 1KSP EPI Engineered Polymers Silicone Polyurea Dispersion
Bakelite® EP 8414 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage
Abatron Metalfix-PH™ Aluminum-Filled, Structural Adhesive Putty; High Temperature Paste

PABCI1 / 21963

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.