MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Eastman TamiSolve® NxG-PS Solvent
Categories: Fluid; Solvent

Material Notes: TamiSolve™ NxG-PS is a high-boiling, dipolar aprotic solvent. TamiSolve NxG-PS has good solvency for a wide range of compounds and has high chemical and thermal stability. TamiSolve NxG-PS has an established performance in various pharmaceutical applications in small molecules and peptides synthesis. In many applications it can be used to replace NMP or NEP (N (m)ethylpyrrolidone), DMAc as well as other solvents like dimethyl sulfoxide (DMSO) and Acetonitrile. As opposed to NMP and NEP, TamiSolve NxG-PS is not classified as developmental toxin.

Applications

  • Pharmaceutical chemicals
Key Attributes
  • Pharmaceutical processing and synthesis

Information provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.960 g/cc
pH 7.6510% solution in water
Viscosity 4.00 cP
Molecular Weight 141.21 g/mol
Vapor Pressure 9.87e-9 atm
Surface Tension 67.31 dynes/cm1% aqueous solution
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 1.98 J/g-°C
Thermal Conductivity 121 W/m-K
Melting Point <= -75.0 °CFreezing Point
Boiling Point 241 °C
Flash Point 108 °CClosed Cup
Ignition Temperature 212 °CAutoignition
 
Descriptive Properties
Hansen Solubility Parameters17.8 (MPa)½Dispersion
 20.5 (MPa)½Total
 5.9 (MPa)½Hydrogen Bonding
 8.2 (MPa)½Polar
Heat of Combustion35580 kJ/kg

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM4175 / 323798

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.