MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Total PSI 740 Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Polystyrene 740 is an impact polystyrene designed for extrusion and injection molding.

It is especially suitable for extrusion thermoforming applications requiring high glass and high stiffness, such as food service disposable. A unique combination of thermal characteristics favors 740 for fast injection cycles in high gloss small appliance and electronics application.

Information provided by Total Petrochemicals, Inc.

Key Words: Impact strength
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 4.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 4300 psiASTM D638
Elongation at Yield 45 %ASTM D638
Tensile Modulus 340000 psiASTM D638
Flexural Strength 8300 psiASTM D790
Flexural Modulus 370 ksiASTM D790
Izod Impact, Notched 1.90 ft-lb/inASTM D256
Falling Dart Impact 10.42 ft-lbASTM D3029
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 203 °FHeat Distortion, Annealed; ASTM D648
Vicat Softening Point 210 °FASTM D1525
 
Optical PropertiesOriginal ValueComments
Gloss 90 %60°; ASTM D523

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NOVA Chemicals Sclair® 11J1 Octene LLDPE Film Resin
Total PSI 825EX Polystyrene
NOVA Chemicals Sclair® FP120-D Octene LLDPE Film Resin
NOVA Chemicals Surpass® FPs117-C Octene Copolymer sLLDPE Film Resins
Total PSC 1540(AS) Crystal Polystyrene

PFIM911 / 38316

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.