MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Toray TOYOLAC™ ABS Resin PX10-X07 ABS/PC Alloy
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: ABS/PC Alloy, PC+ABS.

General Toyolac™ Notes: TOYOLAC™ ABS is a versatile thermoplastic consisting of acrylonitrile, butadiene, and styrene and it has unique set of properties combining strength, lightness, and aesthetics. TOYOLAC™ is widely used in both industrial and household goods due to its excellent mechanical, chemical, electrical properties, and superior processability.

Information provided by Toray Resin Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.12 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cm23°C/50% RH; Toray Method
Melt Flow 29 g/10 min
@Load 9.99 kg,
Temperature 240 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 114
@Temperature 23.0 °C
50% RH; ASTM D785
 114
@Temperature 23.0 °C
ISO 2039-2
Tensile Strength 52.0 MPaASTM D638
 57.0 MPa
@Temperature 23.0 °C
ISO 527-1,2
Elongation at Break 50 %ASTM D638
 50 %
@Temperature 23.0 °C
ISO 527-1,2
Flexural Strength 79.0 MPaASTM D790
 84.0 MPa
@Temperature 23.0 °C
ISO 178
Flexural Modulus 2.10 GPaASTM D790
 2.18 GPa
@Temperature 23.0 °C
50% RH; ISO 178
Izod Impact, Notched 123 J/m
@Thickness 3.20 mm,
Temperature -30.0 °C
V-notched; ASTM D256
 333 J/m
@Thickness 12.7 mm,
Temperature 23.0 °C
V-notched; ASTM D256
 580 J/m
@Thickness 3.20 mm,
Temperature 23.0 °C
V-notched; ASTM D256
Charpy Impact, Notched 60.0 kJ/m²
@Temperature 23.0 °C
V-Notched; ISO 179
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 80.0 µm/m-°CASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 101 °CISO 75-1,2
 108 °CUnannealed; ASTM D648
Vicat Softening Point 115 °C
Flammability, UL94 HB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTORAY9243 / 248932

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.