MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Trinseo Magnum™ 9010 ABS, High Gloss  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ABS resin are available in a wide range of melt flow rates, impact strength and heat resistance for both high and low gloss applications manufactured by injection molding, sheet or profile extrusion and thermoforming.

The MAGNUM 9000 series of high gloss ABS resins are designed to offer a wide range of impact strengths and melt flow rates to meet the needs of the durables injection molding markets. The 9000 series products offer typical Izod impact strength values from 210 to 400 J/m and melt flow rates ranging from 2.5 to 7.0 g/10min. The gloss values are typically greater than 95% on the 60. Gardner scale for the highest gloss resins and greater than 90% for those products having a broader range of gloss.

MAGNUM 9010 ABS resin is one of the highest gloss resins with a medium impact strength and high flow. MAGNUM 9010 is used primarily in injection molding durable applications like housewares and computer equipment where this level of processability is required.

Data provided by Dow Chemical.

Key Words: Poly(Acrylonitrile Butadiene Styrene)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccASTM Data
Melt Density 0.882 g/cc
Linear Mold Shrinkage 0.0055 cm/cm
Melt Flow 7.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM Data
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 107
Tensile Strength, Ultimate 35.9 MPaASTM Data
Tensile Strength, Yield 48.3 MPaASTM Data
Elongation at Break 45 %ASTM Data
Elongation at Yield 2.4 %ISO Data
Tensile Modulus 2.41 GPaASTM Data
Izod Impact, Notched 2.14 J/cmASTM Data
Charpy Impact Unnotched 9.00 J/cm²ISO Data, Low Temp
 NBISO Data
Charpy Impact, Notched 0.600 J/cm²ISO Data, Low Temp
 1.90 J/cm²ISO Data
Instrumented Impact Total Energy 45.0 J
@Temperature 23.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 92.0 µm/m-°C
@Temperature 20.0 °C
ISO data
Specific Heat Capacity 2.03 J/g-°C
Thermal Conductivity 0.128 W/m-K
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °CUnannealed; ASTM Data
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °CUnannealed; 104°C (219°F) annealed; ASTM Data
Vicat Softening Point 108 °C
 
Optical PropertiesOriginal ValueComments
Gloss 95 %Gardner Gloss, 60°

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trinseo Magnum™ 9020 ABS, High Gloss
Trinseo Magnum™ 9030 ABS, High Gloss
Trinseo Magnum™ 9035 ABS, High Gloss
Trinseo Magnum™ 8391 MED Acrylonitrile Butadiene Styrene (ABS) Resin
Covestro Makroblend® UT-640 G Polycarbonate + Polyester Blend

PZZDW100 / 34331

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.