MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Type 332 Austenitic Stainless Steel, Annealed Plate, Sheet, Strip, UNS N08800
Categories: Metal; Ferrous Metal; Stainless Steel; T 300 Series Stainless Steel

Material Notes:

Information provided by Industeel, ATI, Carlson. and the references(s).

Key Words: ASTM B 409
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.027 g/cc0.2900 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 515 MPa74700 psi
Tensile Strength, Yield 210 MPa30500 psi
Elongation at Break 30 %30 %
Modulus of Elasticity 196 GPa28400 ksitypical of UNS N08800
Poissons Ratio 0.340.34
Shear Modulus 73.0 GPa10600 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000990 ohm-cm0.0000990 ohm-cm
Magnetic Permeability 1.00921.0092at 200 Oe
Curie Temperature -115 °C-175 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  14.2 µm/m-°C
@Temperature 20.0 - 90.0 °C
7.89 µin/in-°F
@Temperature 68.0 - 194 °F
 16.0 µm/m-°C
@Temperature 20.0 - 250 °C
8.89 µin/in-°F
@Temperature 68.0 - 482 °F
 16.7 µm/m-°C
@Temperature 20.0 - 500 °C
9.28 µin/in-°F
@Temperature 68.0 - 932 °F
Specific Heat Capacity 0.500 J/g-°C0.120 BTU/lb-°F
Thermal Conductivity 11.6 W/m-K80.5 BTU-in/hr-ft²-°F
Melting Point 1357 - 1385 °C2475 - 2525 °F
Solidus 1357 °C2475 °F
Liquidus 1385 °C2525 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.30 %0.30 %
Carbon, C 0.030 %0.030 %
Chromium, Cr 20.5 %20.5 %
Copper, Cu 0.20 %0.20 %
Iron, Fe 46 %46 %as balance
Manganese, Mn 1.0 %1.0 %
Nickel, Ni 31 %31 %
Phosphorus, P 0.020 %0.020 %
Silicon, Si 0.40 %0.40 %
Sulfur, S 0.010 %0.010 %
Titanium, Ti 0.30 %0.30 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
330 Stainless Steel, annealed plate
347 Stainless Steel, annealed, plate
348 Stainless Steel, annealed
348 Stainless Steel, annealed, plate
409 Stainless Steel

MQ332f / 172140

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.