MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
MRC Polymers EMAREX™ 400 GF33 Nylon 6/6, 33% Glass Fiber Filled  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes:
  • Available in Black only
  • Can be UV and Heat Stabilized
Property data for DAM samples.

Information provided by MRC Polymers Inc.

Key Words: PA66
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.39 g/ccASTM D792
Filler Content 31 - 35 %ASTM D2584
Water Absorption 1.0 %ASTM D570
Relative Viscosity 50 cPASTM D789
Linear Mold Shrinkage 0.0030 in/inASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 101ASTM D785
Tensile Strength at Break 24656 psiASTM D638
Elongation at Break 2.0 %ASTM D638
Flexural Strength 31.0 ksiASTM D790
Flexural Modulus 1200 ksiASTM D790
Izod Impact, Notched 1.30 ft-lb/in
@Temperature 22.8 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 509 °FASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 471 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 450 °FASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 550 - 570 °F
Middle Barrel Temperature 530 - 540 °F
Front Barrel Temperature 520 - 530 °F
Nozzle Temperature 540 - 560 °F
Melt Temperature 520 - 560 °F
Mold Temperature 150 - 250 °F
Drying Temperature 180 - 200 °FDuring prolong interruptions the hopper dryer temperature should be reduced to 65ºC or lower.
Dry Time 4 - 6 hourUntil they reach 0.13% or less moisture level. If bags were left exposed for 3 or more hours, they may not need drying. If exposed to moisture for longer period of time, such as days, they may need 16hrs to dry
Moisture Content <= 0.14 %
Dew Point <= 0.000 °F
Drying Air Flow Rate 0.800 - 1.00 ft³/min (CFM)per lb/hour resin processed
Injection Pressure 10000 - 20000 psi
Back Pressure 0.000 - 50.0 psi
Cushion 0.250 in
Screw Speed 30 - 90 rpm
 
Descriptive Properties
DryerMultiple desiccant chambers and leak free pipes
Fill RateModerate-Fast
Hold Pressure40-60% of injection pressure
Packing Pressure50-75% of injection pressure

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Capron® 5233G 33% Glass-Filled Nylon 66 (Dry)
Celanese Zytel® 105F BK010 PA66
Avient Nymax™ GF 600 A 33 HS Black 22 1 Nylon 6 with 33% Glass Fiber
Omni Plastics OmniLon™ PA6/6 GR33 LM BK2000 Nylon 6/6, 33% Glass reinforced
Domo TECHNYL® B 218L V30 Black 44 N PA66, 30% glass fiber, DRY

PMRC007 / 89436

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.