System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
ASTM A463 Aluminum-Coated Steel, Type I, Drawing Quality, Special Killed
Categories:
Metal
;
Ferrous Metal
;
ASTM Steel
;
Carbon Steel
;
Low Carbon Steel
Material Notes:
Aluminum-coated type 1 steel, coils or cut sheet
Coated with aluminum-silicon alloy by hot dip process
Used for combustion chambers, exhaust systems, heat exchangers and reflectors, ovens, grills, and appliances
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
7.80
g/cc
Typical of ASTM Steel
Coating Weight
2790
g/m²
@Thickness 0.380 mm
3780
g/m²
@Thickness 0.510 mm
4780
g/m²
@Thickness 0.640 mm
5780
g/m²
@Thickness 0.760 mm
6770
g/m²
@Thickness 0.890 mm
7770
g/m²
@Thickness 1.02 mm
8760
g/m²
@Thickness 1.14 mm
9760
g/m²
@Thickness 1.27 mm
10760
g/m²
@Thickness 1.40 mm
11750
g/m²
@Thickness 1.52 mm
12750
g/m²
@Thickness 1.65 mm
13740
g/m²
@Thickness 1.78 mm
14740
g/m²
@Thickness 1.90 mm
15720
g/m²
@Thickness 2.03 mm
16730
g/m²
@Thickness 2.16 mm
17730
g/m²
@Thickness 2.29 mm
18720
g/m²
@Thickness 2.41 mm
19720
g/m²
@Thickness 2.54 mm
20710
g/m²
@Thickness 2.68 mm
21710
g/m²
@Thickness 2.79 mm
22710
g/m²
@Thickness 2.92 mm
23500
g/m²
@Thickness 3.02 mm
Mechanical Properties
Original Value
Comments
Modulus of Elasticity
200
GPa
Typical Carbon Steel
Bulk Modulus
160
GPa
Typical for Steel
Poissons Ratio
0.29
Typical Carbon Steel
Shear Modulus
80.0
GPa
Typical for Steel
Electrical Properties
Original Value
Comments
Electrical Resistivity
0.0000170
ohm-cm
Typical Carbon Steel
Thermal Properties
Original Value
Comments
CTE, linear
12.0
µm/m-°C
Typical Carbon Steel
Specific Heat Capacity
0.470
J/g-°C
Typical Carbon Steel
Thermal Conductivity
52.0
W/m-K
Typical Carbon Steel
Component Elements Properties
Original Value
Comments
Carbon, C
<= 0.10 %
Iron, Fe
99.67 %
as balance
Manganese, Mn
<= 0.50 %
Phosphorus, P
<= 0.025 %
Sulfur, S
<= 0.035 %
References
for this datasheet.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
ASTM A463 Aluminum-Coated Steel, Type I, Drawing Quality
ASTM A463 Aluminum-Coated Steel, Type I, Commercial Quality
ArcelorMittal AS60 Aluminized steel
Armacell Okabell® ASD Aluminized Steel
ArcelorMittal AS80 Aluminized steel
MSA463IDSK / 142777
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.