MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lord Adhesives Chemlok® 8800 Adhesive
Categories: Polymer; Adhesive

Material Notes: LORD Chemlok® 8800 adhesive is a one-coat, aqueous (water-based) adhesive used for bonding silicone rubber, EPDM, HNBR, XHNBR, AFLAS, VAMAC and other peroxide-cured materials. With good resistance to hot oils, hot water and other fluids, Chemlok 8800 adhesive is suitable for use in the manufacture of gaskets, seals and NVH components.

Features: requires only a single coat for most applications, reducing labor, inventory and shipping costs. uses water for dilution; provides reduced VOC emissions. bonds a wide range of compounds to many rigid substrates, such as zinc phosphatized steel, copper, nylon and aluminum. provides good resistance to high temperature fluid environments.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.11 - 1.17 g/cc0.0403 - 0.0424 lb/in³
Solids Content 28 - 32 %28 - 32 %by weight
Brookfield Viscosity 5.0 - 100 cP
@Temperature 25.0 °C
5.0 - 100 cP
@Temperature 77.0 °F
Brookfield LVT, Spindle 2, 30 rpm
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 93.0 °C>= 199 °FSeta
 
Processing PropertiesMetricEnglishComments
Shelf Life 3.00 Month3.00 Monthfrom shipment date, refrigerated in original, unopened container. Do not freeze
 
Descriptive Properties
AppearanceBeige Liquid
SolventsDeionized Water

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLORD9062 / 232451

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.