MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
SABIC SABIC® LDPE 2008N0 PE (Global)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: SABIC® LDPE 2008N0 is a LDPE tubular grade without additives. SABIC® LDPE 2008N0 is produced using SABIC Clean Tubular Reactor (CTR) Technology with typically high purity. Application SABIC® LDPE 2008N0 is typically used as carrier resin for masterbatch and compounding applications. This product is not intended for and must not be used in any pharmaceutical/medical applications.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.920 g/ccASTM D1505
Melt Flow 7.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 10 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ml/10 min; ISO 1133
 28 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ISO 1133
 33 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ml/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 40ISO 868
Tensile Strength at Break 10.0 MPaSpeed of testing: 50 mm/min; ISO 527/1A
Tensile Strength, Yield 8.00 MPaSpeed of testing: 50 mm/min; ISO 527/1A
Elongation at Break 120 %Speed of testing: 50 mm/min; ISO 527/1A
Tensile Modulus 130 MPaSpeed of testing: 50 mm/min; ISO 527/1A
Izod Impact, Notched (ISO) 45.0 kJ/m²ISO 180/A
 9.00 kJ/m²
@Temperature -30.0 °C
ISO 180/A
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 125 J/gDIN 53765
Melting Point 107 °CDIN 53765
Deflection Temperature at 0.46 MPa (66 psi) 43.0 °CBased on injection moulded test specimens,Conditioning of test specimen: temp. 23 °C, relative humidity 50 %, 24 hours; ISO 75-2
Vicat Softening Point 89.0 °Cat 10 N (VST/A); ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10952 / 244419

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.