MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger Tecaform™ UD Blue Ultra Detectable Acetal Copolymer (POM)
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Material Notes: TECAFORM® UD Blue is an Ultra Detectable acetal copolymer designed specifically for applications in the food industry. High speed food production lines detect particulate matter in the food product one of three ways; Using optical scanners, metal detection equipment, or X-ray equipment. TECAFORM® UD Blue is the first engineering thermoplastic that will show up regardless of the scanning method used.

Features:

  • Food contact blue in color
  • High visibility of filler
  • Detectable by X-ray or metal detection equipment
  • Plastic chunks as small as 3mm thick detected using standard metal detection equipment
  • Plastic shavings to 1mm thick detected using standard metal detection equipment
  • Easily machined

Information Provided by Ensinger, Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.61 g/ccASTM D790
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 89ASTM D785
Tensile Strength, Yield 8450 psiASTM D638
Elongation at Break 7.9 %ASTM D638
Tensile Modulus 400000 psiASTM D638
Flexural Strength 13780 psiASTM D790
Flexural Modulus 459000 psiASTM D790
Compressive Strength 12650 psiat 10% deformation; ASTM D695
Compressive Modulus 260000 psiASTM D695
Izod Impact, Notched 0.680 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 320 °FASTM D3418
Maximum Service Temperature, Air 212 °FLong Term; UL746B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CENTROPLAST CENTRODAL MD Polyoxymethylene, Magnetically Detectable
DuPont Mobility and Materials Delrin® FG400MTD BLA079 POM-MED(Fe)
BASF Ultradur® B 6550 PBT
BASF Ultradur® B 6550 LN PBT
BASF Ultradur® B 6550 L PBT

PENSIN997 / 135396

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.