MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Saint-Gobain COHRlastic® R10490 Medium Fluorosilicone Sponge Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Foam

Material Notes: Flexible, compressible COHRlastic silicone closed cell sponge is designed for high-performance gasketing, thermal shielding, vibration mounts and press pads. It is available in six constructions. R10490 fluorosilicone sponge rubber can be used as a gasket where it is necessary to contain fluids that would degrade normal silicone sponge and solid materials (special order basis).
Specification Notes: Meets Specifications: MIL-R-6130 Type II, Grade A. All data based on a 0.0625 inch test sample.(Other thicknesses available.)
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0200 lb/in³ASTM D3574
Water Absorption <= 5.0 %ASTM D1056
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 180 psiASTM D412
Elongation at Break 125 %ASTM D412
Compressive Strength 15.0 psi
@Temperature 23.0 °C
ASTM D1056
Compression Set 25 %ASTM D1056
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 145 V/mil
 
Thermal PropertiesOriginal ValueComments
CTE, linear 180 µin/in-°F
@Temperature 20.0 - 177 °C
Specific Heat Capacity 0.300 BTU/lb-°F
Thermal Conductivity 0.750 BTU-in/hr-ft²-°F
 
Descriptive Properties
ColorBlue

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Fluorosilicone Rubber (FMQ, FVMQ, FSi)
Rogers Arlon 31140R020 0.020" (0.508 mm) Uncured Fluorosilicone Rubber on Release Carrier
ATG s.r.l. FVMQ Fluorosilicone Rubber
Dow Silastic® LS 4-9038 FLUOROSILICONE RUBBER
BCC Products BC 84 PVA Parting

PSTGQZ258 / 68772

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.