MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Michelman® Michem® Emulsion 71731MOD Anionic paraffin emulsion
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Anionic paraffin emulsion

Usage: Michem® Emulsion 71731MOD is an additive designed to provide excellent water resistance especially at higher temperatures. Michem® Emulsion 71731MOD is also very effective in providing durability in auto polish formulations.

We serve many markets through Michem® Emulsion, including: paint & coatings; fiberglass; inks and overprint varnishes; floor care; wood finishes; automotive care products; building products; carpets; die lubricants; fruit and vegetable coatings; textiles and urethane foam

Food Contact Information when manufactured in the USA:
FDA:
175.105: Components of adhesives
176.170: Components of paper and paperboard in contact with aqueous and fatty foods.
176.180: Components of paper and paperboard in contact with dry foods

Information provided by Michelman®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.960 - 0.980 g/cc0.960 - 0.980 g/cc
Volatiles 68 - 70 %68 - 70 %
pH >= 7.0>= 7.0Recommended pH of system
 8.5 - 9.58.5 - 9.5
Brookfield Viscosity <= 200 cP<= 200 cPSpindle # 2, rpm 60
 
Descriptive Properties
AppearanceWhite, low viscosity liquid
Emulsifier ChargeAnionic
Solids TypeParaffin

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Michelman® Michem® Emulsion 34935 Anionic paraffin/ethylene acrylic acid wax emulsion
Michelman® Hydrolube™ 723 Paraffin wax emulsion
Evonik VESTOWAX® H 2050 MG Hard Paraffin Wax
Evonik VESTOWAX® SH 105 Powder Paraffin Wax
Michelman® Michem® Emulsion 47950 Nonionic paraffin emulsion

WMICHEL102 / 135019

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.