MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Oxford Polymers Oxtron PPS-XT-40GF PPS, 40% Glass Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Polyphenylene Sulfide (PPS)

Material Notes: Product Description: Glass Fiber (40% Reinforced), Polyphenylene sulfide injection molding grade based alloy.

Processing and Delivery Form: Pellets and Injection Molding

Appearance: Natural off-white, brown or Black

Information provided by Oxford Polymers

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.54 g/ccASTM D792
Water Absorption at Saturation 0.020 %ASTM D570
Linear Mold Shrinkage, Flow 0.0030 in/in
@Thickness 3.17 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 23000 psiASTM D638
Elongation at Break 1.0 %ASTM D638
Flexural Strength 32000 psiASTM D790
Flexural Modulus 1.80e+6 psiASTM D790
Izod Impact, Notched 1.40 ft-lb/in
@Thickness 3.17 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 465 °FUnannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Melt Temperature 540 - 610 °F
Mold Temperature 200 - 325 °F
Drying Temperature 275 °F
Dry Time 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Oxford Polymers Oxnilon 66-15-IMP Impact Modified Nylon 66 for Injection Molding
Oxford Polymers Oxnilon 66-13GF 13% Glass Fiber Filled Nylon 66 for Injection Molding
Oxford Polymers Stranox PA6/ST/45% Glass Fiber Reinforced Nylon 6, Impact Modified
Oxford Polymers Stranox PA6/45% Glass Fiber Reinforced Nylon 6
Oxford Polymers Stranox PA6/30% Glass Fiber Reinforced Nylon 6

POXF025 / 178455

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.