MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lanxess Keltan® 4455 Ethylene-Propylene Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Amorphous ethylene-propylene rubber with medium ENB (ethylidene norbornene) content and a medium Mooney viscosity at 50 phr oil extension. The high molecular weight allows for high filling levels, and it improves collapse resistance during extrusion. Typical applications can be found in low hardness profiles and molded goods.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.870 g/cc0.0314 lb/in³
Mooney Viscosity 46
@Temperature 125 °C
46
@Temperature 257 °F
(1+4); ISO 289
Storage Temperature >= 30.0 °C>= 86.0 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 36.0 Month36.0 Month
 
Descriptive Properties
Content4.3 percentENB, ASTM D6047
 50 phrOil, ISO 1407
 55 percentEthylene, ASTM D3900

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lanxess Keltan® 3050 Ethylene-Propylene Rubber
Lanxess Keltan® 2470L Ethylene-Propylene Rubber
Lanxess Keltan® 3973 Ethylene-Propylene Rubber
Lanxess Keltan® 5465Q Ethylene-Propylene Rubber
Lanxess Keltan® 2450S Ethylene-Propylene Rubber

PLANY8565 / 208958

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.