MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Refractory Metals

CMW® ELKON 100M Pure Molybdenum  (discontinued **)
Categories: Metal; Nonferrous Metal; Molybdenum Alloy; Refractory Metal; Pure Element

Material Notes: This material has been rebranded as NAECO® ELKON® 100M.

Molybdenum (ELKON® 100M) is a refractory metal that resembles tungsten in many respects. Its hardness, melting, and boiling temperatures are only slightly lower than those of tungsten are. The electrical and thermal conductivity of the two metals is essentially the same. It is fabricated into electrical contacts by slicing discs from rods and brazing them to nickel-plated steel backings, which may be in the form of rivets, screws, or stampings. In atmospheres of inert gasses or vacuum, molybdenum contacts can handle currents of several amperes. Here it has good resistance to welding and electrical erosion because of its refractory metal characteristics. It is readily wet by mercury to form a low resistance contact and is used extensively in mercury switches. It does not contaminate the mercury because it does not react chemically with it. Molybdenum oxidizes more readily than tungsten and, therefore, is seldom used in air applications. If used in air, it is generally limited to 1 ampere and several hundred volts. In certain vibrating contact applications, low mass contacts are desirable, and molybdenum is selected because of its low density. Because of its low expansion characteristic, it is used in non-contact applications such as bases for semiconductor devices. It is also used for faces on resistance welding electrodes.

Information provided by CMW Inc.

Vendors: PLANSEE SE: Whether it's high temperatures, aggressive chemicals or extreme mechanical loading: PLANSEE supplies a suitable product solution in refractory metals or composite materials. As the world market leader in powder metallurgically produced high performance materials we combine outstanding materials knowledge with profound applications and technology know-how. Visit us at www.plansee.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 10.22 g/cc0.3692 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell A 5858
Tensile Strength, Ultimate 585 MPa84800 psi
Modulus of Elasticity 324 GPa47000 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000520 ohm-cm0.00000520 ohm-cm33 % IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 5.35 µm/m-°C
@Temperature 100 °C
2.97 µin/in-°F
@Temperature 212 °F
Thermal Conductivity 142 W/m-K985 BTU-in/hr-ft²-°F
Melting Point 2622 °C4752 °F
Boiling Point 4800 °C8670 °F
 
Component Elements PropertiesMetricEnglishComments
Molybdenum, Mo 100 %100 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NCMW079 / 15892

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.