MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Dow™ 621I LDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Extrusion Grade

Material Notes: Product Description: DOW LDPE 621I Resin is a low density polyethylene resin intended for foam and blown film applications requiring high melt strength.
  • Specialty resin designed for high melt strength applications
  • Provides excellent bubble stability

Complies with: US FDA 21 CFR 177.1520©2.2a; Canadian HPFB No Objections. Consult the regulations for complete details.

Availability: North America

Additive: Antiblock: No; Processing Aid: No; Slip: No

Agency Ratings: FDA 21 CFR 177.1520©2.2; Canadian HPFB No Objections

Form: Pellets

Processing Method: Blown Film; Foam Processing

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc0.0332 lb/in³ASTM D792
Melt Flow 2.3 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.3 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 11.7 MPa
@Thickness 0.0508 mm
1690 psi
@Thickness 0.00200 in
ASTM D882
Film Tensile Strength at Yield, TD 11.0 MPa
@Thickness 0.0508 mm
1600 psi
@Thickness 0.00200 in
ASTM D882
Film Elongation at Break, MD 450 %
@Thickness 0.0508 mm
450 %
@Thickness 0.00200 in
ASTM D882
Film Elongation at Break, TD 620 %
@Thickness 0.0508 mm
620 %
@Thickness 0.00200 in
ASTM D882
2% Secant Modulus  0.166 GPa
@Thickness 0.0508 mm
24.1 ksi
@Thickness 0.00200 in
MD; ASTM D882
 0.208 GPa
@Thickness 0.0508 mm
30.2 ksi
@Thickness 0.00200 in
TD; ASTM D882
Elmendorf Tear Strength MD 320 g
@Thickness 0.0508 mm
320 g
@Thickness 0.00200 in
ASTM D1922
Elmendorf Tear Strength TD 190 g
@Thickness 0.0508 mm
190 g
@Thickness 0.00200 in
ASTM D1922
Dart Drop Test 96.0 g
@Thickness 0.0508 mm
0.212 lb
@Thickness 0.00200 in
ASTM D1709A
Film Tensile Strength at Break, MD 21.8 MPa
@Thickness 0.0508 mm
3160 psi
@Thickness 0.00200 in
ASTM D882
Film Tensile Strength at Break, TD 19.7 MPa
@Thickness 0.0508 mm
2850 psi
@Thickness 0.00200 in
ASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 108 °C226 °F
Vicat Softening Point 92.2 °C198 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 16.1 %
@Thickness 0.0508 mm
16.1 %
@Thickness 0.00200 in
ASTM D1003
Gloss 40 %
@Thickness 0.0508 mm
40 %
@Thickness 0.00200 in
45°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 218 °C425 °FExtrusion
Blow-up Ratio (BUR) 2.52.5
 
Descriptive Properties
Film Puncture Resistance43 ft-lb/in32.0 mil
Film Toughness1700 ft-lb/in3MD, 2.0 mil, ASTM D882
 1709 ft-lb/in3TD, 2.0 mil, ASTM D882

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDOWF470 / 311163

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.