SI 1000 is a surface insensitive cyanoacrylate adhesive that is used in applications that require faster cure speeds, on parts that are dry, and on parts that may be acidic. The SI Series bonds a wide range of similar and dissimilar surfaces. The SI Series provides exceptional performance in a wide range of applications. ABS NBR Acrylic Neoprene Aluminum Nitrile Bakelite Polyester Brass Porcelain Fiberglass PVC Latex Steel Leather Wood.Information provided by Chemical Concepts™. |