MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Petropol Tenopom® B3 P5 S2 MF NTLA016 PR323 POM, Dry
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Product Description: High Flow, Polyacetal Copolymer

Resin ID (ISO 1043): POM-s
Additive: PTFE, Silicone
Processing: Injection Molding, Extrusion
Color: Natural, Opaque

Information provided by Petropol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.43 g/ccASTM D792
Water Absorption 0.33 %
@Temperature 50.0 °C,
Time 86400 sec
Immersion; ASTM D570
Linear Mold Shrinkage 0.017 - 0.018 cm/cmASTM D955
Melt Flow 11 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 130ASTM D785
Tensile Strength 28.0 MPa
@Temperature 80.0 °C
ASTM D638
 35.0 MPa
@Temperature 60.0 °C
ASTM D638
 49.0 MPa
@Temperature 23.0 °C
ASTM D638
 68.0 MPa
@Temperature -40.0 °C
ASTM D638
Elongation at Break 15 %
@Temperature -40.0 °C
ASTM D638
 23 %
@Temperature 23.0 °C
ASTM D638
 56 %
@Temperature 60.0 °C
ASTM D638
 81 %
@Temperature 80.0 °C
ASTM D638
Modulus of Elasticity 0.500 GPa
@Temperature 80.0 °C
ASTM D790
 0.700 GPa
@Temperature 60.0 °C
ASTM D790
 1.70 GPa
@Temperature 23.0 °C
ASTM D790
 4.50 GPa
@Temperature -40.0 °C
ASTM D790
Tensile Modulus 500 MPa
@Temperature 80.0 °C
ASTM D638
 700 MPa
@Temperature 60.0 °C
ASTM D638
 1600 MPa
@Temperature 23.0 °C
ASTM D638
 3400 MPa
@Temperature -40.0 °C
ASTM D638
Flexural Modulus 2700 MPaASTM D790
Izod Impact, Notched 50.0 J/mASTM D256
Izod Impact, Unnotched 490 J/mASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmASTM D257
Surface Resistance 1.00e+16 ohmASTM D257
Dielectric Constant 3.7ASTM D150
Dielectric Strength 19.0 kV/mmASTM D149
Dissipation Factor 0.0060
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Melting Point 170 °C
Deflection Temperature at 0.46 MPa (66 psi) 165 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 99.0 °CASTM D648
Vicat Softening Point 160 °C
@Load 5.10 kg
ASTM D1525
Flammability, UL94 HB
 
Processing PropertiesOriginal ValueComments
Processing Temperature 190 - 215 °CMolding
Mold Temperature 80.0 - 100 °C
Drying Temperature 80.0 °C
Dry Time 3.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPETROPOL393 / 313301

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.