MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont™ 5025 Silver Conductor
Categories: Other Engineering Material; Ceramic/Metallic Coating

Material Notes: DuPont 5025 is one of several commercially available printed silver conductors that can be used to fabricate low voltage circuitry on flexible or rigid substrates. It can be printed with manual, semi-automatic, and reel-to-reel screen print equipment.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 68 - 72 %68 - 72 %
Filler Content 0.00 %0.00 %Silver (Ag)
Particle Size 1.0 µm1.0 µm
Viscosity 20000 - 30000 cP20000 - 30000 cP
Thickness 12.0 - 15.0 microns0.472 - 0.591 mil
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 0.012 - 0.015 ohm0.012 - 0.015 ohm
 
Processing PropertiesMetricEnglishComments
Cure Time 1.00 - 5.00 min0.0167 - 0.0833 hour
 
Descriptive Properties
AdhesionNo Ag transfer after 3M Scotch Tape #600
Binder SystemProprietary
Conductive Filler TypeSilver (Ag)
Material TypeReady-To-Use Formulation
Recommended SubstratesPolyester, Polyimide, Paper, Epoxy Glass
Solvent SystemCarbitol Acetate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 6061-T6; 6061-T651
5025 Aluminum Composition Spec
Alclad Aluminum 6061-T6, T651
Alclad Aluminum 6061-O

PFLEXCM27 / 179429

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.