MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
HT Materials NHU® 21610F PPS Resin for Compression Molding Application
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: NHU® polyphenylene sulfide (PPS) is a semicrystalline high performance thermoplastic with an excellent balance of properties. It is stiff, strong, hard, tough, and has outstanding chemical and oxidative resistance. It retains these properties at temperatures well above 200°C, i.e., its continuous service temperature extends to 240°C. It absorbs little moisture and is both dimensionally stable and inherently flame retardant. It also has excellent electrical properties, is highly impermeable to most liquids and gases, has minimal creep, even at elevated temperatures, and flows well in molding to fill long, thin and complex parts.

Information supplied by HT Materials Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles 0.350 %
@Treatment Temp. 300 °C,
Time 3600 sec
Melt Flow 100 g/10 min
@Load 5.00 kg,
Temperature 316 °C
ISO 1133
Ash 0.300 %
@Treatment Temp. 750 °C
ISO 3451
 
Descriptive Properties
Supply FormPowder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHTMAT923 / 326125

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.