MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Copper Alloy, UNS C64751, H06 Temper, Strip
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Extra Hard

Fabrication Properties: Excellent Suitability – Soldering, Brazing, Spot Weld, Seam Weld, Butt Weld, Capacity for Being Cold Worked; Good Suitability – Oxyacetylene Welding, Gas Shielded Arc Welding, Coated Metal Arc Welding; Fair Suitability – Capacity for Being Hot Formed

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.86 g/cc0.320 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers >= 255
@Load 3.00 kg
>= 255
@Load 6.62 lb
Tensile Strength 848 MPa123000 psiTypical
 800 - 903 MPa116000 - 131000 psi
Tensile Strength, Yield 758 - 876 MPa110000 - 127000 psi0.2% Offset
 820 MPa119000 psi0.2% Offset, Typical
Elongation at Break >= 1.0 %>= 1.0 %
Tensile Modulus 131 GPa19000 ksi
Modulus of Rigidity 49.25 GPa7143 ksiCalculated
Poissons Ratio 0.330.33
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000510 ohm-cm0.00000510 ohm-cm34% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.3 µm/m-°C
@Temperature 20.0 - 300 °C
9.61 µin/in-°F
@Temperature 68.0 - 572 °F
Thermal Conductivity 13.7 W/m-K95.0 BTU-in/hr-ft²-°F
Melting Point 1050 - 1075 °C1922 - 1967 °F
Solidus 1050 °C1922 °F
Liquidus 1075 °C1967 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 95.5 - 96.9 %95.5 - 96.9 %As Balance
Nickel, Ni 2.5 - 3.1 %2.5 - 3.1 %
Phosphorus, P <= 0.020 %<= 0.020 %
Silicon, Si 0.50 - 0.90 %0.50 - 0.90 %
Tin, Sn 0.10 - 0.40 %0.10 - 0.40 %
Zinc, Zn <= 0.10 %<= 0.10 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC64751x2 / 292234

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.