MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Silberline Sparkle Silver® 3122-AR
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Sparkle Silver® 3122-AR is a coarse, non-leafing, acid stain resistant aluminum flake pigment. It is characterized by high sparkle, a white face color and deep flop. The main applications are high quality industrial finishes and bicycle and automotive component paints. A regular purity version, Sparkle Silver® 3622, is also available.

Applications: Automotive

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.79 g/cc1.79 g/cc
Bulk Factor 0.0660.066
Volatiles 22 %22 %
Particle Size 36 µm36 µm
Particle Mesh Size <= 325 Mesh<= 325 Mesh1% retained
 
Descriptive Properties
SolventsMineral Spirits/High Flash

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Potters Industries Conduct-O-Fil® AG-SL150-16-TRD Silver-coated Hollow Ceramic Spheres
Overview of materials for Silver Alloy
Silver Aluminum Selenide, AgAlSe2
Silver-Copper Eutectic Alloy (72Ag-28Cu; UNS P07720; AWS BAg-8), Cold Drawn then Annealed at 250°C (480°F)
MetalTek MTEK 12% Ni 410 Cast UNS C97300 Nickel-Silver

ESIBER002 / 5757

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.