MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Westlake EF522 12% Ethylene Vinyl Acetate Copolymer  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Film Grade

Material Notes: Westlake ELEVATE™ EF522 is an ethylene vinyl acetate copolymer with 12% VA. EF522 is designed for blown and cast films requiring excellent optics and low heat seal initiation. High melt strength makes EF524 an excellent choice for profile extrusions, molding, and foaming applications requiring medium VA content..

    Application/Uses
  • Flexible packaging films
  • Peelable seals, adhesive layers
  • Injection and blow molding
  • Profile extrusions, tubing, wire & cable

This resin grade complies with 21 CFR, section 177.1350.

Key Words: Excellent optics and low heat seal initiation. 12% EVA
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.933 g/cc0.0337 lb/in³D1505
Vinyl Acetate Content 12 %12 %
Thickness 33.0 microns1.30 milThickness Tested
Melt Flow 2.5 g/10 min2.5 g/10 minD1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 300 %300 %D882
Film Elongation at Break, TD 800 %800 %D882
Dart Drop 7.27 g/micron185 g/milD1709
Dart Drop Test 240 g0.529 lbD1709
Film Tensile Strength at Break, MD 26.9 MPa3900 psiD638
Film Tensile Strength at Break, TD 22.1 MPa3210 psiD638
1% Secant Modulus, MD 72.4 MPa10500 psiD882
1% Secant Modulus, TD 79.3 MPa11500 psiD882
 
Thermal PropertiesMetricEnglishComments
Melting Point 94.0 °C201 °FDSC Peak; D3418
Vicat Softening Point 70.0 °C158 °FD1525
 
Optical PropertiesMetricEnglishComments
Haze 2.3 %2.3 %D1003
Gloss 84 %84 %at 45°; D2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature <= 193 °C<= 379 °FBlown Film
 <= 210 °C<= 410 °FCast Film
Blow-up Ratio (BUR) 2.52.5As Tested
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
processFilm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lushan EV1050G2 EVA Film for Encapsulating Solar modules, High Transmittance
Lushan EV1050G1 EVA Film for Encapsulating Solar modules, Ultra Fast Cure
LG Chemical SEETEC ES440 Ethylene Vinyl Acetate
LG Chemical SEETEC EF443 Ethylene Vinyl Acetate
LG Chemical SEETEC EF321 Ethylene Vinyl Acetate

PWESF8928s / 146112

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.