MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Chosun Refractories SFC-165 High-Alumina Castable
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes:

Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture  0.010791 GPa
@Temperature 110 °C,
Time 86400 sec
1.5651 ksi
@Temperature 230 °F,
Time 24.0 hour
 0.011772 GPa
@Temperature 1000 °C,
Time 10800 sec
1.7074 ksi
@Temperature 1830 °F,
Time 3.00 hour
 0.012753 GPa
@Temperature 1350 °C,
Time 10800 sec
1.8497 ksi
@Temperature 2460 °F,
Time 3.00 hour
Compressive Strength  53.9 MPa
@Treatment Temp. 110 °C,
Time 86400 sec
7820 psi
@Treatment Temp. 230 °F,
Time 24.0 hour
Cold Crushing Strength
 78.5 MPa
@Treatment Temp. 1000 °C,
Time 10800 sec
11400 psi
@Treatment Temp. 1830 °F,
Time 3.00 hour
Cold Crushing Strength
 83.4 MPa
@Treatment Temp. 1350 °C,
Time 10800 sec
12100 psi
@Treatment Temp. 2460 °F,
Time 3.00 hour
Cold Crushing Strength
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 1650 °C3000 °Flimited
Shrinkage  -0.0300 %
@Temperature 110 °C,
Time 86400 sec
-0.0300 %
@Temperature 230 °F,
Time 24.0 hour
 0.12 %
@Temperature 1350 °C,
Time 10800 sec
0.12 %
@Temperature 2460 °F,
Time 3.00 hour
 
Component Elements PropertiesMetricEnglishComments
Al2O3 61 %61 %
SiO2 34 %34 %
 
Descriptive Properties
Installation MethodSelf Flowing
Material Required for Estimating (kg/m3)2,450
Water Required for Casting(%)7.3-7.7

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
MarkeTech AO 98 Aluminum Oxide Ceramic Substrate, 98% Purity
Iron (II) Bromide, FeBr2
H.C. Starck Amperit® 740.3 Aluminum Oxide (Al2O3)
Ferro Aluminum Oxide P890
Chosun Refractories TD-R75 Monolithic Refractories for Ladle and Tundish

CCHOS191 / 124135

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.