MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultraform® N2650 Z6 POM + PUR
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Description: Elastomer-modified injection molding grade for applications requiring highest impact strength together with low stiffness.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.850 g/cc0.0307 lb/in³
Density 1.33 g/cc0.0480 lb/in³ISO 1183
Water Absorption 0.80 %0.80 %ISO 62
Moisture Absorption at Equilibrium 0.20 %0.20 %ISO 62
Melt Flow 9.31 g/10 min
@Load 2.16 kg,
Temperature 190 °C
9.31 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 38.0 MPa5510 psi50 mm/min; ISO 527-1/-2
Elongation at Break 44 %44 %50 mm/min, Nominal; ISO 527-1/-2
Elongation at Yield 19 %19 %50 mm/min; ISO 527-1/-2
Tensile Modulus 1.20 GPa174 ksiISO 527-1/-2
Charpy Impact Unnotched  24.0 J/cm²
@Temperature -30.0 °C
114 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.900 J/cm²
@Temperature -30.0 °C
4.28 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 2.00 J/cm²
@Temperature 23.0 °C
9.52 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
Tensile Creep Modulus, 1000 hours 500 MPa
@Strain <=0.5 %
72500 psi
@Strain <=0.5 %
ISO 899-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+11 ohm-cm1.00e+11 ohm-cmIEC 60093
Surface Resistance 1.00e+12 ohm1.00e+12 ohmIEC 60093
Dielectric Constant 4.3
@Frequency 1e+6 Hz
4.3
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.025
@Frequency 1e+6 Hz
0.025
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VTest Solution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 140 µm/m-°C
@Temperature 23.0 - 55.0 °C
77.8 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1/-2
Melting Point 166 °C331 °FISO 11357-1/-3
Maximum Service Temperature, Air 100 °C212 °F
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C167 °FISO 75-1/-2
Decomposition Temperature >= 240 °C>= 464 °F
Ignition Temperature 320 - 340 °C608 - 644 °FASTM D1929
 
Processing PropertiesMetricEnglishComments
Processing Temperature 200 °C392 °FHopper Throat
Zone 1 200 °C392 °FFeed zone
Zone 2 200 °C392 °FCompression
Zone 3 200 °C392 °FMetering-zone
Zone 4 200 °C392 °FNozzle
Melt Temperature 200 °C392 °FOptimal
 190 - 215 °C374 - 419 °FInjection molding
Mold Temperature 60.0 °C140 °FOptimal
 60.0 - 80.0 °C140 - 176 °FInjection molding
Drying Temperature 100 °C212 °F
Dry Time 3 hour3 hour
 
Descriptive Properties
Commercial StatusEurope
Peripheral Screw Speed<0.3 m/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultraform® N2644 Z9 POM + PUR
BASF Ultraform® N2650 Z4 POM + PUR
BASF Ultraform® N2640 Z2 POM + PUR
3M Scotch-Weld™ EZ250015 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive
3M Dyneon™ LTFE 6400Z Low Temperature Fluoroelastomer

PBASG0166 / 131799

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.