MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lubrizol Hipscon™ M-530 Static Control Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Molded, Unreinforced

Material Notes: Hipscon™ M-530 is a conductive, carbon black filled, polystyrene available as extruded sheet and compound. Thermoformed trays are lightweight and easily formed into deep pockets that maintain uniform static protection. The M-530, high in stiffness, insures uniform pocket formation in critical performance application. Hipscon™ M-530 sheet is available in custom extruded gauges from 0.012 to 0.080 inch and widths of 10 to 48 inches. Product is typically provided as rollstock with a smooth surface finish.

Features:

  • Superior impact strength
  • High degree of stiffness
  • High Gloss

Applications:

  • Tape & reel
  • Electronic component packaging
  • Component handling trays

Data provided by Noveon, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.09 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 3500 psiASTM D638
Elongation at Break 16 %ASTM D638
Tensile Modulus 200000 psiASTM D638
Flexural Modulus 315000 psiASTM D790-92
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+7 ohm-cm50% RH; ASTM D257
Surface Resistance 10000 ohmESD S11.11
Surface Resistivity per Square 1e+0550% RH; ASTM D257
Static Decay <= 0.010 secFTMS-101C; 12% R.H., (+5000 V to 50 V)
 <= 0.010 secFTMS-101C; 12% R.H., (-5000 V to -50 V)
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °CASTM D648
 
Optical PropertiesOriginal ValueComments
Gloss 20 %60°; Back
 35 %60°; Front
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNOVEON06 / 55327

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.