MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Titanium Ti-6Al-2Sn-4Zr-6Mo (Ti-6-2-4-6) STOA
Categories: Metal; Nonferrous Metal; Titanium Alloy; Alpha/Beta Titanium Alloy

Material Notes: Information provided by Allvac and the references. Solution Treated 870ºC, Overaged 705ºC. Alpha-Beta Alloy.

Characteristics: High strength at elevated temperatures, heat-treatable, good hardenability, weldable.

Applications: Intermediate-temperature jet engine applications. Blades, discs, spacers, seals.

Forms typically available: Billet, bar, plate and sheet.

4 other heat treatments of this alloy are listed in MatWeb.

Key Words: Ti-6246; Titanium 6-2-4-6; UNS R56260
Vendors:
TITANIUM ENGINEERS is your source for high strength, NACE titanium alloys, with a full range of stock sizes and sizes made to order. Our in-house metallurgical experts ensure the best alloy selection and process titanium to meet unique customer specifications. Please visit our website www.TitaniumEngineers.com for more information or call us at +1 281 265 2910 (USA) or +44 (0) 1675 464200 (UK).

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 4.65 g/cc0.168 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 351351Estimated from Rockwell C.
Hardness, Knoop 382382Estimated from Rockwell C.
Hardness, Rockwell C 3838
Hardness, Vickers 367367Estimated from Rockwell C.
Tensile Strength, Ultimate 1120 MPa162000 psi
 1160 MPa168000 psisheet
Tensile Strength, Yield 1040 MPa151000 psi
 1110 MPa161000 psisheet
Elongation at Break 15 %15 %Value for sheet reported 12%
Reduction of Area 42 %42 %
Tensile Modulus 114 GPa16500 ksi
Poissons Ratio 0.330.33Typical for alpha-beta titanium alloy.
Fatigue Strength  260 MPa
@# of Cycles 1.00e+7
37700 psi
@# of Cycles 1.00e+7
notched
 620 MPa
@# of Cycles 1.00e+7
89900 psi
@# of Cycles 1.00e+7
Unnotched
Shear Modulus 42.9 GPa6220 ksiCalculated from typical values.
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000190 ohm-cm0.000190 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear  8.60 µm/m-°C
@Temperature 20.0 °C
4.78 µin/in-°F
@Temperature 68.0 °F
 9.90 µm/m-°C
@Temperature 205 °C
5.50 µin/in-°F
@Temperature 401 °F
 10.4 µm/m-°C
@Temperature 540 °C
5.78 µin/in-°F
@Temperature 1000 °F
Specific Heat Capacity 0.500 J/g-°C0.120 BTU/lb-°F
Thermal Conductivity  7.70 W/m-K
@Temperature 23.0 °C
53.4 BTU-in/hr-ft²-°F
@Temperature 73.4 °F
 13.5 W/m-K
@Temperature 540 °C
93.7 BTU-in/hr-ft²-°F
@Temperature 1000 °F
Melting Point 1595 - 1675 °C2903 - 3047 °F
Solidus 1595 °C2903 °F
Liquidus 1675 °C3047 °F
Beta Transus 935 °C1720 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 6.0 %6.0 %
Carbon, C <= 0.040 %<= 0.040 %
Iron, Fe <= 0.15 %<= 0.15 %
Molybdenum, Mo 6.0 %6.0 %
Nitrogen, N <= 0.040 %<= 0.040 %
Oxygen, O <= 0.12 %<= 0.12 %
Tin, Sn 2.0 %2.0 %
Titanium, Ti 82 %82 %
Zirconium, Zr 4.0 %4.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Titanium Ti-6Al-2Sn-4Zr-6Mo (Ti-6-2-4-6) BSTA
Titanium Ti-6Al-2Sn-4Zr-6Mo (Ti-6-2-4-6) STA-2
Titanium Ti-6Al-2Sn-4Zr-6Mo (Ti-6-2-4-6) Annealed
Titanium Ti-6Al-2Sn-4Zr-6Mo (Ti-6-2-4-6) STA-1
ATI Allvac® 6-2-4-6 Titanium Alloy, Heat Treatment: 885°C (1625°F) + Age

MTP624 / 14237

Metalmen Sales

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.