Desmoderm KEN Granular is a one-component polyester polyether urethane based on an aromatic diisocyanate. Uses: Desmoderm KEN Granular is used as the base component in the polyurethane coagulation process. Desmoderm KEN Granular is suitable for use in the manufacture of materials for shoe linings, shoe uppers, bags/luggage and clothing, as well as in the manufacture of nubuk products. Information provided by Covestro |