MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
UNS C81700, Copper Casting Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy; Copper Casting Alloy

Material Notes:

Casting methods recommended for this alloy: Centrifugal, Continuous, Investment, Permanent Mold, Plaster, and Sand.

Applications: Electrical and/or thermal conductors used as structural members where strength and hardness greater than that of UNS C8100-8110 are required. Also used in place of UNS C81500 where electrical and or thermal conductivities can be sacrificed for hardness and strength.Inactive per the Copper Development Association.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.85 g/ccEstimated
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 2173000 kg; heat treated
Tensile Strength, Ultimate 634 MPaheat treated
Tensile Strength, Yield 469 MPaheat treated
Elongation at Break 8.0 %heat treated
Machinability 30 %UNS C36000 (free-cutting brass) = 100%
 
Component Elements PropertiesOriginal ValueComments
Beryllium, Be 0.40 %
Cobalt, Co 0.90 %
Copper, Cu >= 94.25 %
Nickel, Ni 0.90 %
Silver, Ag 1.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
UNS C80100, Copper Casting Alloy
UNS C80500, Copper Casting Alloy
UNS C80900, Copper Casting Alloy
UNS C81400, Copper Casting Alloy
UNS C81500, Copper Casting Alloy

MC81700b1 / 11860

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.