MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

MMCC Copper/Graphite Fiber GC 7-340 Metal Matrix Composite  (discontinued **)
Categories: Metal; Metal Matrix Composite; Nonferrous Metal

Material Notes: Discontinuous graphite fiber copper product primarily used for electronic thermal management applications. Lightweight, high damping, stiffer than aluminum, matched cte, easily machined and plated, superior thermal conductivity, non-carcinogenic.

As power densities increase, reducing or eliminating thermal mismatch strains in an electronic assembly improve system reliability and performance. MMCC’s graphite fiber reinforced aluminum and copper products cover a wide spectrum of substrate and IC packaging requirements.

Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC).

MatWeb has no current information on Metal Matrix Cast Composites (MMCC).

Key Words: Cu/Gr
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 6.80 g/cc0.246 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 62.1 MPa9010 psi
Modulus of Elasticity 89.0 GPa12900 ksiYoung's Modulus
Flexural Yield Strength 160 MPa23200 psiFlexural Strength
Compressive Yield Strength 83.7 MPa12100 psi
Ultimate Compressive Strength 196 MPa28400 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000436 ohm-cm0.00000436 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 7.40 µm/m-°C
@Temperature 20.0 °C
4.11 µin/in-°F
@Temperature 68.0 °F
x-y direction
Thermal Conductivity 200 W/m-K1390 BTU-in/hr-ft²-°Fz direction
 300 W/m-K2080 BTU-in/hr-ft²-°Fx-y directions

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
MMCC Al/Al2O3 Particulate Aluminum Matrix Composite
MMCC Aluminum/Al2O3 55p Aluminum Matrix Composite
MMCC Aluminum/SiC 55p Aluminum Matrix Composite
Applied Composites 120 Polyester SMC
DWA 6091/SiC/20p-T6 Aluminum SiC Metal-Matrix-Composite (Al MMC)

NZMMC5 / 20037

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.