MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Abatron AboCast/AboCure 8508-1/8508-1 Primerless, High-Solids Epoxy  (discontinued **)
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Primerless, high-solids epoxy structural paint for concrete, wood, metal and composite surfaces. 2-component system in standard and custom colors.

Suggested Uses: Protective and decorative painting of floors and most rigid surfaces in industrial, construction, marine and general environment. Primer and color base for polyurethanes and other paints. Protection against water, salt, weathering, fuels, oils, alkalis, detergents, diluted acids. Renewing or skid-proofing concrete, metal and wood floors. Outstanding for wear resistance, hardness, flexibility, versatility, permanence. Can be applied with spray, brush, or roller.

Processing:

Ratio by volume: 1/1

Cure Schedule: Room temperature cure 6-8 hours for handling, 2-3 days for full physical properties, and 6-7 days for full resistance properties. Optional high temperature bake 35-45 minutes at 150°F, 20-30 minutes at 200°F, or 15-20 minutes at 250°F. Baking is useful for fast optimum results.

Information provided by Abatron.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 10.5 lb/gal
Solids Content 64 - 65 %
Viscosity Measurement 73K.U.
 
Processing PropertiesOriginal ValueComments
Pot Life 480 - 720 min
 
Descriptive Properties
Pencil Hardness3Overnight

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PABKW013 / 22054

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.