MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
NeXolve LaRC™-CP1 Conductive Black Polyimide
Categories: Polymer; Film; Thermoset; Polyimide, TS; Polyimide, Thermoset Film

Material Notes: Lower RF loss than other black and conductive black polyimides.

NeXolve’s Conductive Black LaRC™-CP1 Polyimide is filled with carbon nanoparticles to produce a conductive black polyimide material with lower RF loss than other black and conductive black polyimides. CP1 is a space rated colorless polyimide material designed by NASA and further developed by NeXolve.

Conductive Black LaRC-CP1 Polyimide exhibits very high optical density (>4) and light blocking. It is useful in applications requiring static dissipation, as it exhibits ESD-level surface resistivity (105-109 ohms/sq).

Conductive Black LaRC-CP1 Polyimide exhibits high emissivity, surpassing 0.80 at 1 mil thickness. Additionally, it can be sprayed and cast into a variety of shapes, using low-temperature curing (<100°C) for solvent removal.

Conductive Black LaRC-CP1 Polyimide is manufactured in continuous rolls of 0.1, 0.25, 0.50, and 1.0 mil thickness.

Information Provided by NeXolve Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Stress 140 MPa
@Thickness 0.0500 mm
ASTM D882-02
Elongation at Break 6.7 %
@Thickness 0.0500 mm
ASTM D882-02
Tensile Modulus 6.30 GPa
@Thickness 0.0500 mm
ASTM D882-02
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 1e+05 - 1.00e+9 ohm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 40.0 µm/m-°C
@Thickness 1.00 mm,
Temperature 125 - 175 °C
ASTM E831-06
Glass Transition Temp, Tg 263 °CDSC; ASTM E1356-03
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 0.00 %
@Thickness 0.0130 mm
Solar Transmittivity; ASTM E903-96
 0.00 %
@Thickness 0.0250 mm
Solar Transmittivity; ASTM E903-96
 0.00 %
@Thickness 0.0500 mm
Solar Transmittivity; ASTM E903-96
Reflection Coefficient, Visible (0-1) 0.050
@Thickness 0.0130 mm
Solar Reflectivity; ASTM E903-96
 0.050
@Thickness 0.0250 mm
Solar Reflectivity; ASTM E903-96
 0.050
@Thickness 0.0500 mm
Solar Reflectivity; ASTM E903-96
 
Descriptive Properties
Solar Absorptivity0.950.5 mil thickness; ASTM E903-96
 0.951.0 mil thickness; ASTM E903-96
 0.952.0 mil thickness; ASTM E903-96

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NeXolve LaRC™-CP1 Polyimide
NeXolve Clear Optionox® Polyimide Film/Coating
NeXolve Thermalbright® C Polyimide Film
NeXolve Thermalbright® N Polyimide Film
NeXolve UV Blocking Optionox® Polyimide Film/Coating

PNEXOL907 / 171861

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.