Description: Thermoplastic elastomer SBS rubber T-171 is an oil-extended styrene-butadiene-styrene triplex block copolymer especially for shoes with high molecular weight and radiation type. Its oil-extended rate is 33%, and the styrene content of SBS polymer T-171 is 40%. Application: Shoes/Compounding SBS(T-171): 40 PS: 8 SiO2: 7 Naphethenic Oil: 7 K-resin: 3 Information provided by BEC Materials, LLC |