MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Danquinsa DANTHANE® 125K-20F Compound Coating
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: The TPU compound DANTHANE_ 125K-20F Compound is a melt coating raw material based on TPU/PTFE in the form of granules. This type is specially suitable for the melt calendaring process. For the coating of transport elements such as conveyor belts, coating of drive sections (flat drive belts) and for the coating of technical textiles, which are acting for the production of transport boxes, big-bags, hoses and others it can be used here the specific characteristics of the product DANTHANE_ 125K-20F-Compound This special compound will be used for coatings, which must be protected against contamination and which must show a high tendency to slide.

Application: DANTHANE_ 125K-20F Compound is needed by the hot melt coating of industrial textiles. The coated textiles and industrial woven fabrics are being used to produce transport and drive elements, flexible beverage containers and containers for solid goods, health and safety protection, etc. For an optimal processing DANTHANE_ 125K- 20F-Compound is pre-plasticized by the use of an extruder. The hot melt is transferred directly to the hot melt calender rolls. The pre-plasticizing is also possible direct on the heated calender rolls. The hot melt of DANTHANE_ 125K-20F-Compound can be applied to transfer paper to produce films with a different strength. The TPU-films can be laminated to the supporting textiles. For impregnation and as bonding agent (adhesive), to this textiles we recommend our special polyurethane adhesives of the DANCOLL_ range. Especially we recommend the product DANCOLL_ 245-10. A direct hot melt coating is also possible with DANTHANE_ 125K-20FCompound. DANTHANE_ 125K-20F-Compound is further used as a binder by the production of TPU-colour and additive masterbatches. DANTHANE_ 125K-20F-Compound is applied in the shape of granules or grinded into powders depending on the kind of processing.

Information provided by Danquinsa GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³DIN 53.479
Melt Flow 65 - 95 g/10 min
@Load 10.0 kg,
Temperature 190 °C
65 - 95 g/10 min
@Load 22.0 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8686DIN 53.505
Tensile Strength 30.0 MPa4350 psiDIN 53.504
Elongation at Break 500 %500 %DIN 53.504
100% Modulus 5.50 MPa798 psiDIN 53.504
200% Modulus 6.00 MPa870 psiDIN 53.504
300% Modulus 8.50 MPa1230 psiDIN 53.504
Abrasion 2525[mm³]; DIN 53.516
Compression Set  30 %
@Temperature 23.0 °C,
Time 252000 sec
30 %
@Temperature 73.4 °F,
Time 70.0 hour
DIN 53.517
 80 %
@Temperature 70.0 °C,
Time 86400 sec
80 %
@Temperature 158 °F,
Time 24.0 hour
DIN 53.517
 
Thermal PropertiesMetricEnglishComments
Melting Point 140 - 145 °C284 - 293 °FKofler
Softening Point 120 - 125 °C248 - 257 °FKofler
 140 - 145 °C284 - 293 °FCharacteristic of the film
Glass Transition Temp, Tg -27.0 °C-16.6 °FDSC; DIN 51.007
 
Processing PropertiesMetricEnglishComments
Processing Temperature 120 - 180 °C248 - 356 °FFilm processing temperature
 160 - 170 °C320 - 338 °FCompression zone
 175 - 185 °C347 - 365 °FMetering zone
Feed Temperature 150 - 160 °C302 - 320 °F
Die Temperature 175 - 185 °C347 - 365 °F
Drying Temperature 90.0 - 100 °C194 - 212 °F
Dry Time 2.00 hour2.00 hour
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
AspectWhite colored pearl granule(RAL 9011)
 white, elasticCharacteristic of the film

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDANQ135 / 294555

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.