MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Acudel® 79000 Polyphenylsulfone, Modified (PPSU, Modified)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphenylsulfone (PPSU)

Material Notes: Acudel 79000 is a modified polyphenylsulfone developed specifically for cost-effective aircraft interior applications. Through the use of a proprietary flame retardant package, this resin offers low heat release, low smoke generation and low toxic gas emissions, thereby complying with the FAA regulation 14CFR Part 25.853 Appendix F. In addition, it has excellent impact resistance and meets typical industry requirements for resistance to aerospace fluids, even under stress. Acudel 79000 exhibits behavior similar to Radel® polyphenylsulfone and therefore offers a practical solution for many aircraft applications. Acudel 79000 was developed for extrusion fabrication to produce articles such as profiles, shapes and tubes. This grade has been formulated for colored applications where there is low UV exposure and is suggested for use in applications where coatings, paints or other secondary surface decoration will protect the part from direct UV exposure.

Extrusion Notes: Screw Compression Ratio: 2.5:1 to 3.5:1 Metering Flights: 4 to 10 Take-off Roll Hot Oil Temp: 400° to 450°F Normal Roll Temp: 370° to 420°F

Information provided by Solvay Specialty Polymers.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.34 g/ccvaries with resin color.; ASTM D792
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 380 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 71.0 MPaASTM D638
Elongation at Break 33 %ASTM D638
Tensile Modulus 2410 MPaASTM D638
Flexural Strength 109 MPaASTM D790
Flexural Modulus 2690 MPaASTM D790
Izod Impact, Notched 100 J/mASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 207 °CUnannealed; ASTM D648
Smoke Density <= 5.0
@Time 360 sec
Dmax; ASTM F814/E662
 
Processing PropertiesOriginal ValueComments
Zone 1 327 °C
Zone 5 382 °C
Die Temperature 327 - 371 °C
Melt Temperature 343 - 382 °C
Drying Temperature 177 °C
Dry Time 5.00 hour
 
Descriptive Properties
Agency RatingsFAA FAR 25.853a
 FAA FAR 25.853d
AppearanceColors Available
AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
FeaturesDetergent Resistant
 Flame Retardant
 Good Chemical Resistance
 Good Thermal Stability
 Good Toughness
 High Heat Resistance
 Hydrolytically Stable
 Low Smoke Emission
 Low Toxicity
FormsPellets
GenericPPSU, Modified
OSU Peak Heat Release Rate< 55.0 kW/m²FAR 25, AppF
OSU Total Heat Release< 10.0 kW·min/m²FAR 25, AppF
Processing MethodExtrusion
 Profile Extrusion
 Sheet Extrusion
 Thermoforming
RoHS ComplianceRoHS Compliant
Toxic Gas Emissions (ppm)< 1BSS 7239/ATS 1000/ABD 0031; HCl
 < 1BSS 7239/ATS 1000/ABD 0031; HCN
 < 1BSS 7239/ATS 1000/ABD 0031; HF
 < 1BSS 7239/ATS 1000/ABD 0031; NO+NO2
 < 1BSS 7239/ATS 1000/ABD 0031; SO2
 < 10BSS 7239/ATS 1000/ABD 0031; CO
UsesAircraft Applications
 Aircraft Interiors
Vertical Burn - 60 second< 7.62 cmLength; DMS 1510
 0 hrFlame Time; DMS 1510

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y7501 / 135582

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.