MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ExxonMobil Exterex™ A32 Synthetic Fluid
Categories: Fluid; Lubricant

Material Notes: Product Description: Esterex™ Adipate Esters are API category Group V fluids. These esters have excellent low-temperature properties, high viscosity indices, good lubricating properties and low volatilities. Esterex™ Adipate Esters can be used as sole basestocks or blendstocks with other synthetic fluids in many automotive and industrial lubricant applications. These esters are ideal in high-temperature conditions, such as reciprocating air compressors, where discharge valve cleanliness is required.

Appearance: Bright & Clear

Availability: Africa & Middle East, Asia Pacific, Central America, Europe, North America and South America

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.928 g/cc
@Temperature 15.6 °C
ASTM D4052
Viscosity Measurement 19Index; ASTM D2270
Kinematic Viscosity 985 cSt
@Temperature -40.0 °C
ASTM D445
Kinematic Viscosity at 40°C (104°F) 9.5 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 2.8 cStASTM D445
Evaporation Loss 53 %
@Temperature 205 °C,
Time 23400 sec
ASTM D972
 
Chemical PropertiesOriginal ValueComments
Acid Value <= 0.080[mg KOH/g]; ASTM D974 (mod)
 
Thermal PropertiesOriginal ValueComments
Pour Point -85.0 °FASTM D5950/D97
Flash Point 405 °FCOC; ASTM D92
 460 °FPMCC; ASTM D92
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.4465ASTM D1218
 
Descriptive Properties
Aniline Point<68°FASTM D611
Biodegradation (%)70.2OECD 301F
Color<0.5ASTM D1500
CompositionWater<50 ppm, ASTM D6304 (mod)
Density Correction Factor0.000756 (g/cc)/°CASTM D1250
Elastomer Compatibility (%)-18Fluoroelastomer Hardness Change, ASTM D471
 -18Nitrile Hardness Change, ASTM D471
 -22.4Polyacrylate Elongation Change, ASTM D471
 -23Polyacrylate Hardness Change, ASTM D471
 28.1Fluoroelastomer Volume Change, ASTM D471
 41.3Nitrile Volume Change, ASTM D471
 -42.4Fluoroelastomer Tensile Strength Change, ASTM D471
 -44.9Nitrile Elongation Change, ASTM D471
 -55Polyacrylate Tensile Strength Change, ASTM D471
 -6.7Fluoroelastomer Elongation Change, ASTM D471
 -60.7Nitrile Tensile Strength Change, ASTM D471
 72.8Polyacrylate Volume Change, ASTM D471
Fire Point460°FCOC, ASTM D92
Hydrolytic Stability, TAN Change0.10 mg KOH/gASTM D2619
Kauri-Butanol Value106.5ASTM D1133
Noack Volatility (%)30.3ASTM D5800/DIN 51581
RPVOT>1210 minWith AO, ASTM D2272
 315 minNeat, ASTM D2272

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow UCON™ LB-65 Fluids and Lubricants
ChevronTexaco 5606G Aircraft Hydraulic Oil
Anderol ANDEROL® FGH 22 Synthetic Food Grade Hydraulic Fluid, ISO 22
Phillips 66 Syncon® 32 Synthetic AW Hydraulic Fluid 32
Phillips 66 Syncon® 22 Synthetic AW Hydraulic Fluid 22

PEX99699 / 175935

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.