MC511A is a high strength, glass epoxy laminate that is specially formulated to meet power generation producer’s exacting standards where higher strength at elevated temperatures are required. MC511A is certifiable to MIL-I-24768/3, Type GEB and is halogen free to meet the European restrictions.Information provided by Norplex-Micarta |
Glass Fiber, Epoxy, Micarta, NEMA G-11, ASTM D709 Type IV Grade G-11, MIL-I-24768/3 GEB |