MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Sandvik Sanicro 29 fro OCTG Tube and pipe, seamless
Categories: Metal; Ferrous Metal; Alloy Steel; Austenitic

Material Notes: Sanicro 29 is a high-alloy austenitic stainless steel (CRA) for OCTG down-hole applications in particularly corrosive conditions. The grade is characterized by:
  • Very good resistance to sulphide stress cracking and stress corrosion cracking (SCC) in H2S environments
  • Very high resistance to pitting and crevice corrosion
  • Higher pitting resistance equivalent (PRE) than Sanicro 28 (UNS N08028)
Sanicro 29 is developed specifically for improved localized corrosion resistance where the environment contains high chloride concentrations, CO and H S at high temperatures. Such an environment causes corrosion in lower alloyed materials. Sanicro 29 offers a cost effective solution to such corrosion problems over the more expensive nickel alloys.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.00 g/cc0.289 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C <= 35<= 35Sanicro 29-110
 <= 37<= 37Sanicro 29-125
Tensile Strength, Ultimate >= 795 MPa>= 115000 psiSanicro 29-110
 >= 895 MPa>= 130000 psiSanicro 29-125
Tensile Strength, Yield  760 - 965 MPa
@Strain 0.2 %
110000 - 140000 psi
@Strain 0.2 %
Sanicro 29-110
 860 - 1035 MPa
@Strain 0.2 %
125000 - 150100 psi
@Strain 0.2 %
Sanicro 29-125
Elongation at Break >= 10 %>= 10 %Sanicro 29-125
 >= 11 %>= 11 %Sanicro 29-110
Modulus of Elasticity  174 GPa
@Temperature 300 °C
25200 ksi
@Temperature 572 °F
 182 GPa
@Temperature 200 °C
26400 ksi
@Temperature 392 °F
 190 GPa
@Temperature 100 °C
27600 ksi
@Temperature 212 °F
 195 GPa
@Temperature 20.0 °C
28300 ksi
@Temperature 68.0 °F
Poissons Ratio 0.300.30
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  0.0000100 ohm-cm
@Temperature 150 °C
0.0000100 ohm-cm
@Temperature 302 °F
 0.0000100 ohm-cm
@Temperature 200 °C
0.0000100 ohm-cm
@Temperature 392 °F
 0.0000101 ohm-cm
@Temperature 20.0 °C
0.0000101 ohm-cm
@Temperature 68.0 °F
 0.0000101 ohm-cm
@Temperature 100 °C
0.0000101 ohm-cm
@Temperature 212 °F
 0.0000104 ohm-cm
@Temperature 250 °C
0.0000104 ohm-cm
@Temperature 482 °F
 0.0000111 ohm-cm
@Temperature 300 °C
0.0000111 ohm-cm
@Temperature 572 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  13.0 µm/m-°C
@Temperature 30.0 - 50.0 °C
7.22 µin/in-°F
@Temperature 86.0 - 122 °F
 14.5 µm/m-°C
@Temperature 30.0 - 100 °C
8.06 µin/in-°F
@Temperature 86.0 - 212 °F
 15.0 µm/m-°C
@Temperature 30.0 - 150 °C
8.33 µin/in-°F
@Temperature 86.0 - 302 °F
 15.0 µm/m-°C
@Temperature 30.0 - 200 °C
8.33 µin/in-°F
@Temperature 86.0 - 392 °F
 15.0 µm/m-°C
@Temperature 30.0 - 250 °C
8.33 µin/in-°F
@Temperature 86.0 - 482 °F
 15.0 µm/m-°C
@Temperature 30.0 - 300 °C
8.33 µin/in-°F
@Temperature 86.0 - 572 °F
Specific Heat Capacity  0.460 J/g-°C
@Temperature 20.0 °C
0.110 BTU/lb-°F
@Temperature 68.0 °F
 0.465 J/g-°C
@Temperature 50.0 °C
0.111 BTU/lb-°F
@Temperature 122 °F
 0.480 J/g-°C
@Temperature 100 °C
0.115 BTU/lb-°F
@Temperature 212 °F
 0.490 J/g-°C
@Temperature 150 °C
0.117 BTU/lb-°F
@Temperature 302 °F
 0.495 J/g-°C
@Temperature 200 °C
0.118 BTU/lb-°F
@Temperature 392 °F
 0.505 J/g-°C
@Temperature 250 °C
0.121 BTU/lb-°F
@Temperature 482 °F
 0.515 J/g-°C
@Temperature 300 °C
0.123 BTU/lb-°F
@Temperature 572 °F
Thermal Conductivity  11.0 W/m-K
@Temperature 20.0 °C
76.3 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
 11.0 W/m-K
@Temperature 50.0 °C
76.3 BTU-in/hr-ft²-°F
@Temperature 122 °F
 12.0 W/m-K
@Temperature 100 °C
83.3 BTU-in/hr-ft²-°F
@Temperature 212 °F
 13.0 W/m-K
@Temperature 150 °C
90.2 BTU-in/hr-ft²-°F
@Temperature 302 °F
 14.0 W/m-K
@Temperature 200 °C
97.2 BTU-in/hr-ft²-°F
@Temperature 392 °F
 15.0 W/m-K
@Temperature 250 °C
104 BTU-in/hr-ft²-°F
@Temperature 482 °F
 16.0 W/m-K
@Temperature 300 °C
111 BTU-in/hr-ft²-°F
@Temperature 572 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.020 %<= 0.020 %
Chromium, Cr 27 %27 %
Copper, Cu 1.0 %1.0 %
Manganese, Mn <= 2.5 %<= 2.5 %
Molybdenum, Mo 4.4 %4.4 %
Nickel, Ni 31.5 %31.5 %
Phosphorus, P <= 0.025 %<= 0.025 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.015 %<= 0.015 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NSANDV5250 / 199814

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.