MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Blue River Coatings Low VOC Primer Sealer
Categories: Polymer; Adhesive; Thermoset

Material Notes: BLUE RIVER COATINGS LOW VOC PRIMER SEALER is a high quality, single component primer. Performance obtained is equal or superior to that of single component solvent primers. LOW VOC PRIMER SEALER offers good coverage, excellent durability, and ease of application, as well as being a low VOC and EPA compliant coating.

Enviromental Advantages:BLUE RIVER COATINGS LOW VOC PRIMER SEALER is a low VOC (Volatile Organic Compound), high performance production coating. It is considered non-hazardous by EPA definitions and does not contain lead or chromates. The solid and semi-solid sludge produced in spraying and clean up can be flocculated; dried and sent to a “Class B” landfill. Check with local and state regulations for proper handling.

Characteristics:

  • Excellent exterior durability
  • Excellent hardness/impact resistance
  • Excellent mar and abrasion resistance
  • Excellent adhesion on plastics and gel coat substrates
  • Solvent resistant
  • Can be applied in a wide variety of temperature and humidity conditions without the use of retarders
  • Distilled water is used for reduction
  • Water is used for clean-up
  • Non-Hazardous
  • Air dry or force curing preferred
  • Can be oven baked
  • Wide range of colors
  • Coating will not flash rust on bare metal
  • Shelf life of 1 year
  • Unused paint can be returned to container
  • Non-Flammable
  • Uses

  • Steel
  • Metal
  • Corrosion Resistance – ASTM B117, Good corrosion resistance – Pass at 450 hours. Coating was applied at 1 mil dry and allowed to cure for 15 days at ambient temperatures. Additional corrosion resistance can be achieved when the coated is applied with a higher film build.

  • 1 mil dry – Pass 250-300 hours
  • 2 mil dry – Pass 450 hours
  • 4 mils dry – Pass 600 hours
  • 6+ mils dry – Pass 750 hours
  • Exterior Exposure Test – Coating was applied to steel panel at 1 mil dry and allowed to cure for 15 days at ambient temperatures. Panel was positioned for southern exposure for an indefinite amount of time. After 24 months exposure, panel does not exhibit any blistering, cracking, spot rusting or delamination of film.

    Information provided by Blue River Coatings

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Specific Gravity >= 1.00 g/cc>= 1.00 g/cc
    Density 1.241 g/cc0.04485 lb/in³
    Solids Content 40.62 %40.62 %by volume
     43.2 %43.2 %by weight
    Volatile Organic Compounds (VOC) Content 144 g/l144 g/l
    pH 7.0 - 8.57.0 - 8.5
     
    Mechanical PropertiesMetricEnglishComments
    Impact Test 20.3 J15.0 ft-lbReverse/direct on steel
     
    Thermal PropertiesMetricEnglishComments
    Boiling Point 169 °C336 °F
    Flash Point 65.6 °C150 °F
     
    Processing PropertiesMetricEnglishComments
    Cure Time  10.0 min
    @Temperature 75.0 °C
    0.167 hour
    @Temperature 167 °F
    Recoat, at 50% humidity
     19.8 min
    @Temperature 75.0 °C
    0.330 hour
    @Temperature 167 °F
    Dust Free, at 50% humidity
     30.0 min
    @Temperature 75.0 °C
    0.500 hour
    @Temperature 167 °F
    Dry to handle, at 50% humidity and 75°C
    Shelf Life 12.0 Month12.0 Month
     
    Descriptive Properties
    Evaporation rateSlower than ether
    Pencil HardnessH-HB; ASTM 3363
    Tape AdhesionPass (5B); ASTM D-3359, cross hatch adhesion test after 72 hours submersion and allowed to air dry for 4 hours at 70% humidity and 75°F
    Theoretical Coverage652 ft2 at 1 mil
    Vapor DensityHeavier than air
    Water Submersion72 hours; 70°F – No delamination, peeling, wrinkling, or blistering to unaided eye. Coating was applied to steel panel at 1 mil dry and allowed to cure for 15 days at ambient temperatures.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    WBLUER01 / 74600

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.