System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Axiall 22840 Coax & Telecom Flexible PVC
(discontinued **)
Categories:
Polymer
;
Thermoplastic
;
Vinyl (PVC)
Material Notes:
Non-lead stabilized, Category 5, flexible CMR jacket at 28-30 mils over HDPE inners.
Information provided by Georgia Gulf
Georgia Gulf became Axiall Corporation, which was later acquired by Westlake Plastics. This specific grade is discontinued.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.48
-
1.52
g/cc
1.48
-
1.52
g/cc
ASTM D-792
Mechanical Properties
Metric
English
Comments
Hardness, Shore A
81 - 87
81 - 87
delayed; ASTM D-2240
Tensile Strength, Yield
15.2
MPa
2200
psi
ASTM D-638
Elongation at Yield
235.5 %
235.5 %
Air Aging: 10 days @ 100°C; 30 mil slabs; UL 1581
300 %
300 %
ASTM D-638
100% Modulus
9.17
MPa
@Strain 100 %
1330
psi
@Strain 100 %
ASTM D-638
Thermal Properties
Metric
English
Comments
Brittleness Temperature
-24.0
°C
-11.2
°F
ASTM D-746
Oxygen Index
35.8 %
35.8 %
ASTM D-638
Processing Properties
Metric
English
Comments
Melt Temperature
185
°C
365
°F
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Axiall 1601 Clear 7002 Flexible PVC
Fainplast Compounds GS 54/AM Flexible PVC, Electrical Plugs Lead Free
Axiall 1025-115A Flexible PVC
Fainplast Compounds CL 006 Flexible PVC, Sheathing
Fainplast Compounds KL 50 Flexible PVC, Insulation for High Temperatures Lead Free
PGGUL032 / 41308
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.