MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Eneos 1800B TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Characteristics:
  • Dynamic vulcanized TPO
  • High melt flow and good injection moldability
  • Excellent adhesion with cured rubbers
  • Wide Range of hardness (20-80 (DuroA))
Typical Applications:
  • Corner moldings of weather seals
  • Various types of seals(replacement of urethane foam)

ENEOS has acquired the elastomer product lines from JSR Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.890 g/cc0.890 g/ccISO 1183
Melt Flow 24 g/10 min
@Load 2.14 kg,
Temperature 230 °C
24 g/10 min
@Load 4.72 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 78
@Time 15.0 sec
78
@Time 0.00417 hour
ISO 868
Tensile Strength 3.20 MPa464 psiAdhesion Test with Cured EPDM( Hs70A), 200mm/min.
 8.50 MPa1230 psiISO 37(I)
Elongation at Break 150 %150 %Adhesion Test with Cured EPDM( Hs70A), 200mm/min.
 640 %640 %ISO 37(I)
100% Modulus 3.20 MPa464 psiISO 37(I)
Tear Strength 38.0 kN/m217 pliISO 34 B (a)
Compression Set 59 %
@Temperature 70.0 °C,
Time 79200 sec
59 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -60.0 °C<= -76.0 °F
Shrinkage 0.80 %0.80 %
 
Optical PropertiesMetricEnglishComments
Gloss 50 %50 %ISO 2813

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PJSRC8138 / 295454

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.