MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Momentive Performance Materials GE Silicones IGS3763 Two-Component Insulating Glass Silicone
Categories: Polymer; Thermoset; Silicone

Material Notes: IGS3763 adhesive silicone is an optimized, high-modulus, neutral curing sealant for edge seal applications for gas and air filled structural and non- structural insulating glass units. IGS3763 two-component silicone offers variable work life with fast deep section cure to accommodate scheduling and production needs.

Features: High Modulus, High Elastic Recovery, Fast Cure, Compatibility, Non-flammable.

Applications: Structural Glazing, Silicone Durability, Adhesive. Note: IGS3763 silicone should only be used in the fabrication of insulating glass where the dual seal method of fabrication is used. The moisture vapor transmission rate of silicone sealants is sufficiently high as to preclude their use in the fabrication of single seal insulating glass units. Silicone setting blocks are recommended for direct contact with IGS3763 silicone. Avoid using non-silicone materials (i.e., EPDM, Neoprene) as they could degrade or discolor the secondary seal over time. Avoid IGS3763 to be in contact with or exposed to sealants that evolve acetic acid cure byproduct. Not recommended for water immersion applications.

IGS3767 is the gray equivalent.

Information provided by Momentive Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 g/ccComponent B
 1.47 g/ccMixed; uncured
 1.50 g/ccComponent A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 55ASTM D2240
Tensile Strength 1.00 MPaISO 8339
 1.12 MPaASTM C1135
Tensile Strength, Ultimate 2.10 MPaASTM D412
Tensile Stress at Strain 0.440 MPa
@Strain 10 %
ASTM C1135
 0.700 MPa
@Strain 25 %
ISO 8339
 0.860 MPa
@Strain 25 %
ASTM C1135
Elongation at Break 46 %ASTM C1135
 60 %ISO 8339
Elongation, Ultimate 222 %ASTM D412
Modulus of Elasticity 0.00260 GPaETAG 002
Shear Strength 0.900 MPaASTM C961
Tear Strength 6.61 kg(f)/cmASTM D624, die B
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 300 °FHeat Resistance
 
Processing PropertiesOriginal ValueComments
Tack-Free Time 40.0 - 170 min2X snap time
Shelf Life 12.0 MonthComponent B, when properly stored.
 18.0 MonthComponent A, when properly stored.
 
Descriptive Properties
Accelerated WeatheringExcellent, no degradation.5000 hours
AppearanceThixotropic PasteComponent A
 Thixotropic PasteComponent B
 Thixotropic PasteMixed
ColorBlackComponent B
 BlackCured
 BlackMixed
 GrayComponent A
Consistency / Sag<0.05”Non-sagging
Design Stress in Tension0.15 Mpa
Gas Permeability0.924 g/m2hEN1279-4
Mix Ratio12.5:1As Tested
 8:1 to 11:1Mixed by volume
Resistance to Tearingcategory 1
Snap Time20-85 minutes
Water Penetration23.4 g/m2EN1279-4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMOMEN9925 / 265735

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.