MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Ovako C55 510A Steel, Hardening
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: General Information: C55 is a carbon steel for general purposes found in three variants in EN10083-2. SB C55 meets all three of them. A tight chemical composition ensures repeatable properties
Ovako 510A is an ingot casted steel. High hardness (approx. 60HRC) and high strength can be achieved after hardening due to the relatively high carbon content. The steel is suitable for various type of applications where high strength is needed
Ovako 056K is a low alloyed steel for quench and tempering. Used for machine parts etc. Can be induction or flame hardened
SBC55 is a continuous casted variant

Information provided by Ovako

Key Words: C54, C55E - 1.1203, C55R - 1.1209, 070M55 (BS970), ASTM/SAE 1055, SS 1655, C55R, Cf53, 1.1213
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.80 g/cc0.282 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 700 - 850 MPa
@Thickness 25.0 - 40.0 mm
102000 - 123000 psi
@Thickness 0.984 - 1.57 in
Round bar
Tensile Strength, Yield >= 420 MPa
@Thickness 25.0 - 40.0 mm
>= 60900 psi
@Thickness 0.984 - 1.57 in
Round bar
Elongation at Break 15 %
@Thickness 25.0 - 40.0 mm
15 %
@Thickness 0.984 - 1.57 in
Round bar
Reduction of Area 40 %
@Thickness 25.0 - 40.0 mm
40 %
@Thickness 0.984 - 1.57 in
Round bar
Modulus of Elasticity 210 GPa30500 ksi
Poissons Ratio 0.300.30
Shear Modulus 80.0 GPa11600 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000200 - 0.00000250 ohm-cm0.00000200 - 0.00000250 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 12.0 µm/m-°C
@Temperature 20.0 - 300 °C
6.67 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.460 - 0.480 J/g-°C
@Temperature 50.0 - 100 °C
0.110 - 0.115 BTU/lb-°F
@Temperature 122 - 212 °F
Thermal Conductivity 40.0 - 45.0 W/m-K278 - 312 BTU-in/hr-ft²-°FAmbient temperature
Transformation Temperature 270 °C518 °FMS
 720 °C1330 °FAC1
 750 °C1380 °FAC3
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.48 - 0.55 %0.48 - 0.55 %
Chromium, Cr <= 0.30 %<= 0.30 %
Iron, Fe 97.44 - 98.77 %97.44 - 98.77 %As Balance
Manganese, Mn 0.60 - 0.80 %0.60 - 0.80 %
Molybdenum, Mo <= 0.10 %<= 0.10 %
Nickel, Ni <= 0.30 %<= 0.30 %
Phosphorus, P <= 0.035 %<= 0.035 %
Silicon, Si 0.15 - 0.35 %0.15 - 0.35 %
Sulfur, S <= 0.025 %<= 0.025 %
Vanadium, V <= 0.10 %<= 0.10 %
 
Descriptive Properties
WeldabilityCEV 0.86max
 Pcm 0.66max

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type D3 Tool Steel, oil-quenched from 980°C (1800°F), tempered at 200°C
Ovako 34CrMo4 4130 ASTM A29 Steel
United Cast Bar Unibar 250 Continuously Cast Iron
Rogers Arlon 44570R010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate
Ovako C55 EN 10083-2:2006 (ref) Steel, Hardening

NOVAKO395 / 234694

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.