MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
EMS-Grivory Grilamid® LV-23 ESD PA12-GF23
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, 20% Glass Fiber Filled

Material Notes: Product description: Grilamid LV-23 ESD is a 20% fiber reinforced, anti-static injection molding grade Polyamide 12 (PA12). Grilamid LV-23 ESD is heat stabilized, is easy to process and demold. The inherent color of this product is black. The main features of Grilamid LV-23 ESD are:
  • Electrically conductive/ anti-static
  • Heat stabilized
  • High stiffness and strength
  • Good chemical resistance
  • Good oil resistance
  • High surface quality
  • Good dimensional stability
  • Low density, low weight
Grilamid LV-23 ESD is suitable for the production of injection molded parts in the area of electro/electronics and in the automotive industry for anti-static housings, covers and small components.

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccDry; ISO 1183
Water Absorption 1.0 %Sim. to ISO 62
Moisture Absorption 0.500 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0070 cm/cmISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 75
@Time 15.0 sec
Conditioned; ISO 868
Tensile Strength at Break 95.0 MPaConditioned; ISO 527-1/-2
 110 MPaDry; ISO 527-1/-2
Elongation at Break 3.0 %Dry; ISO 527-1/-2
 5.0 %Conditioned; ISO 527-1/-2
Tensile Modulus 5000 MPaConditioned; ISO 527-1/-2
 5800 MPaDry; ISO 527-1/-2
Charpy Impact Unnotched 40.0 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eU
 70.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eU
Charpy Impact, Notched 6.00 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eA
 8.00 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 100 ohm-cmConditioned; IEC 60093
Surface Resistance 10000 ohmIEC 60093
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 20.0 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 150 µm/m-°CISO 11359-1/-2
Melting Point 178 °C10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 - 120 °CLong Term; ISO 2578
 150 °CShort Term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 150 °CISO 75-1/-2
Deflection Temperature at 8.0 MPa 80.0 °CISO 75-1/-2
Flammability, UL94 HBIEC 60695-11-10
 
Descriptive Properties
AutomotiveFuel systems
FormGranules
ProcessingInjection Molding
Product AttributesHydrolysis resistant
Special CharacteristicsAnti-static
 High impact or impact modified
 Improved heat resistance
 Improved UV resistance (outdoor use)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
EMS-Grivory Grilamid® LV-23H PA12-GF23
A. Schulman ComAlloy Comshield® 120 Copolymer Polypropylene, Electrically Conductive - Carbon Black Filled
Asahi Kasei Thermylene® P6-30FG-0877A 30% Glass Fiber Reinforced, UV Stabilized Polypropylene
Asahi Kasei Thermylene® P6-30FG-0602 30% Glass Fiber Reinforced, UV Stabilized Polypropylene
A. Schulman ComAlloy Comshield® 104 Homopolymer Polypropylene, Electrically Conductive - Carbon Black Filled

PGRH072 / 156781

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.