MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Saint-Gobain CHR® 2345-1 Polyimide Film Backing Silicone Adhesive Pressure Sensitive Tape
Categories: Polymer; Tape; Thermoset; Polyimide, TS; Silicone

Material Notes: CHR® 2345-1 is manufactured from polyimide film with high-temperature adhesive.

Features/Benefits: CHR® 2345-1 and K250 meet the Underwriters Laboratories, Inc. Guide File E66639 and File E51201 respectively with a 180°C temperature rating, and they comply with UL510 for flame retardance.

Applications: CHR® 2345-1 is often used for applications that require holding, insulating, or wrapping. CHR® 2345-1 is chosen for gold finger protection during wave solder applications.
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break 50 %50 %
Tear Strength 5.26 kN/m30.0 pliInitial Tear Strength
Peel Strength 0.270 kN/m1.54 pliAdhesion to Steel
 
Electrical PropertiesMetricEnglishComments
Dielectric Breakdown 6500 V6500 V
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 260 °C500 °F
Minimum Service Temperature, Air -73.3 °C-100 °F
 
Descriptive Properties
ColorAmber

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
UBE UPILEX 25S (25 micron) Polyimide Film
Saint-Gobain CHR® K350 Polyimide Film Backing Silicone Adhesive Pressure Sensitive Tape
Saint-Gobain CHR® 2345-5 Polyimide Film Backing Silicone Adhesive Pressure Sensitive Tape
DuPont™ Kapton® 100HN Polyimide Film, 25 Micron Thickness
CEN® Electronic Material CV Polyimide Film, 2 Mil Thickness

PSTGQZ328 / 68842

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.