MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lubrizol Stat-Rite® X5166 Static Dissipative Polystyrene Compound
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Molded, Unreinforced

Material Notes: Stat-Rite® X5166 is a static dissipative, High-Impact Polystyrene alloy. Stat-Rite® X5166 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD protection. Stat-Rite® IDP alloys retain consistent uniform static dissipation properties when thermoformed into complex tray designs.

Features:

  • Clean: no sloughing, low offgassing, low ionics
  • Consistent ESD properties after thermoforming
  • Carbon-free protection

Applications:

  • Electronic component packaging
  • Tape and reel packaging
  • Electronic assembly trays

Information provided by Noveon, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.06 g/ccASTM D-792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 14.5 MPaASTM D-638-95
Elongation at Break 60 %ASTM D-638-95
Tensile Modulus 0.894 GPaASTM D-638-95
Flexural Modulus 0.894 GPaASTM D-790-95
Izod Impact, Notched 4.00 ft-lb/inASTM D-256-92
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 5.00e+10 ohmASTM D-257
Static Decay 0.30 sec+5000 to 50 V; (12% R.H.); FTMS-101C
 1.5 sec+1000 to 100 V; Charged Plate Monitor (50% R.H.)
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °CASTM D-648-92
Deflection Temperature at 1.8 MPa (264 psi) 62.0 °CASTM D-648-92
Vicat Softening Point 94.0 °CASTM D-1525-95
 
Descriptive Properties
ColorWhite
FillerIDP Alloy

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNOVEON34 / 55460

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.